Page 123 - ProStar Product Guide
P. 123
™
ProStar Metal-Cored Wire
™
StarCore 6LS Wire
SPECIFICATION
E70C-6M H4 per AWS A5.18, ASME SFA 5.18
Wire Dia Package Part No.
0.052" 750 lb (340 kg) drum PRSS279315-713
CHARACTERISTICS
• Clean weld beads with minimal silicon
islands; almost self-peeling
• Weld bead toe lines almost completely
free of silicon deposits
• Better wetting action than solid wire
• Better side wall fusion than solid wire
• Ideal for sheet metal
ProStar StarCore 6LS wire is a metal-cored wire
with fewer silicon islands than other metal-cored
wires; remaining islands are almost self-peeling. Weld
bead toe lines and the weld bead face are nearly
free of silicon deposits reducing cleanup. Combined FILLER METALS
with low spatter rates, StarCore 6LS wire saves time
and money spent cleaning prior to painting, coating
or plating. Recommended for single-pass and multi- ProStar StarCore 6 metal-cored wire offers less
pass welding in both flat and horizontal positions. spatter, cleaner welds and reduced fume levels.
Recommended shielding gas is a mixture of argon
and CO 2, with a minimum of 75% Ar and a maximum
of 92% Ar. Arc characteristics improve with richer
argon gases while spatter and fume levels decrease.
Shielding Gas Welding Positions
75 – 92% Ar/Bal CO2, 35 – 50 cfh Flat and horizontal
Typical Mechanical Properties*
Tensile Strength 90,200 psi (622 MPa)
Yield Strength 80,000 psi (552 MPa)
Elongation 25%
CVN at -0 °F (-18 °C) 50 ft/lb (68 Joules)
CVN at -20 °F (-29 °C) 42 ft/lb (57 Joules)
Typical Undiluted Weld Metal Chemistry
* The data contained herein is based on testing performed under standard
Carbon (C) 0.05 Phosphorus (P) 0.011
laboratory conditions. In normal practice, the results obtained may vary depending
Manganese (Mn) 1.38 Sulphur (S) 0.013 upon welding parameters, weld metal cooling rate, and the base plate being
joined. The user should always test the electrode prior to its application.
Silicon (Si) 0.65 Nickel (Ni) 0.40