What is a HydroStar Blend?

HydroStar Blends Argon, Helium, Argon/Hydrogen

Argon, helium, argon/helium and argon/hydrogen blends are used for a variety of TIG (gas tungsten arc) welding applications. Base material type and thickness, and the desired welding speed influence gas selection. A primary function of the shielding gas is to protect the tungsten electrode from oxidation. The DCEN or DCSP (electrode is negative polarity) power connection is used for carbon steel welding; AC with high frequency is recommended for aluminum.

Argon is recommended for manual welding of all materials. Its easy arc starting characteristics allow excellent control of arc voltage even as arc length varies with manual operations.

Helium is used to join thick plate and metals that rapidly conduct heat, such as aluminum and copper. Helium's high thermal conductivity creates a hotter, broader arc for higher welding speeds and deeper penetration. Arc starting and stability is not as good as argon. Increased gas flow rates and larger diameter electrodes must be used with helium shielding.

HydroStar argon/hydrogen blends from Linde are primarily used with austenitic stainless steels (300 series) and other nickel alloys. Severe weld porosity and cracking may occur if used to join aluminum, copper and most carbon steels. Hydrogen increases the thermal conductivity of the gas blend while providing a reducing atmosphere to improve weld puddle wetting and weld bead cleanliness. Significant increases in travel speed can also be attained. Additions of 2-5% are typically used for manual welding; higher percentages (10-15%) are used in mechanized applications.

Features

  • Argon provides best arc stability/cleaning action
  • Helium provides greater heat input
  • Linde's HydroStar H-5 offers higher heat input and a reducing atmosphere

Benefits

  • First choice for TIG welding/good arc starting
  • Maximum cleaning action (aluminum)
  • Improved puddle fluidity and welding speed
  • Better control of bead shape and distortion
  • Good arc starting and increased heat input
  • Deeper penetration as helium content increases
  • Excellent bead shape and appearance
  • Higher travel speeds on stainless steel; less distortion
  • Excellent as a purge gas. Deeper penetration as helium content increases

Typical Applications

Argon
  • Mild Steel
  • Light Gauge Material
  • Thin aluminum
Linde's HydroStar Blends
  • Stainless Steel Tubing
  • Stainless Steel Food Equipment
  • Railings
  • Aerospace Components

 

Below are comparisons between shielding gas blends over a range of operating conditions. They are intended to provide suggestions for gas blend selection based on the criteria indicated.

hydrostar h5 comparisons

Note: The selection of the appropriate shielding gas can be complex due to the variety of operating variables (base metal chemistry and thickness, transfer type, wire selection and welding position). Consult your Linde representative to help you choose the best gas for your application.

Welding Conditions Table

Wire Diameter (in)ProcessTungsten DiameterCurrent Level (amps)Voltage (volts)*
1/16 to 1/8
Carbon or Stainless Steel
GTAW1/16" diameter tungsten80-150
80-150
80-150
80-150
11-13
13-15
15-17
12-14

* Voltage level for 60 Hz power supply. Add 2-3 volts for 50 Hz models.